Tuesday, January 31, 2023

[MW:33974] Issues with Tacking


Dear Experts,


Please find the attached pictures if there are alternate options for Fit up as tacking has been done directly on the Flange.


Please advise.


Best Regards,

 

Krishna Kamal Nayan  


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---