Dear Experts,
-- We have a Vessel with the following MOC.(API RP 934 C)
Material 1 : SA 387 GR.11 CL.2 + SA 240 GR.347 (3.2 mm Cladded) -80 MM
Material 2 : SA 387 GR.11 CL.2 - 25 mm
Requesting your Technical inputs for PQR establishment.
Regards,
Manikandan