Wednesday, January 11, 2023

[MW:33914] Request for Information

Dear Experts,

It's a very nice platform to gain & share knowledge.

I have a query regarding the weld bead length. What is the maximum weld bead/weave length in Power Piping? (ASME B 31.1)
or 
Is there any thumb rule for weld bead length?

Your idea/advice will be highly welcomed & appreciated.

Be safe & have a healthy Life

Thanks,

Kind Regards,

G.Gughan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB0bcTMUzgWi-7pQvfdjj-e93ChHhYcq93UYgWC3xe9Kv4hnng%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...