Skip to main content

Re: [MW:33856] Stabilizing treatment of SS plate /components

Basically it is performed to form TiC and/ NbC and so no further C available for IGC attack/

Thanks & Regards

J.Gerald Jayakumar




On Monday, 26 December, 2022 at 08:48:47 am IST, 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear  Mr.Prakash,

stabilized heat treament is required for stablized staniless steel only, not for all SS grades.
stabilizing alloys of Like : Nb/Cb, Ti ,Zr & others are speciafiaclly added in the normal SS aloys to avoid senstitization, after solution heat treatement we don't know about whether these stabilzed alloys are setteld in grain boundry or in the core. hence to ensure the stabilized alloys in grain boundry this stabilized heat treatment is essential, as per ASTM A 182 ot ASTM A 351 this stabilized heat teratment is given as subimentary variable for forging & casting respectively. During stabilized heat treatement soaking hour to given as 4 hour (min).          
 
Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India. 


On Thursday, 22 December, 2022 at 08:53:38 am IST, 'Prakash Hegde' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Hi! Friends
Why some of the client spec ask for
Stabilizing treatment (At lower temperature than solution annealing i.e. about 900C) of already solution annealed plate but not Welded SS components

Especially  304H,347,321

Regards
Hegde

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/743927190.1795927.1671599012641%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/709916209.2786676.1671884370625%40mail.yahoo.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...