Skip to main content

Re: [MW:33836] Re: Vanadium composition showing in p91

Gentleman,

SA234 WP22 is for 2.25Cr-1Mo steel

where as P91 is modified 9Cr-1Mo steel with additions of Nb and V which provides higher creep strength at applicable higher temperatures and which differentiates from P9 steel (9Cr-1M0).

See below snap shot

Inline image

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 20 December, 2022 at 08:49:29 am IST, mithlesh kumar <mithleshmech47@gmail.com> wrote:



Sir please read WP22 instead of P91
On Monday, December 19, 2022 at 3:01:56 PM UTC+5:30 kannayeram gnanapandithan wrote:
P/T 91 is CrMov steel
It should have Vanadium  and it is a precipitation hardening elements.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Dec 19, 2022 at 8:43 AM Vishwas Keskar Welding Manager WELDING <vvkes...@gmail.com> wrote:
What is the % Vanadium in that MTC ?
It is trace elements not a deliberate addition for Gr 22  unlike Gr 91 where it it MUST in Gr 91 

Regards

Vishwas IWE
International Welding Engineer 


On Saturday, December 17, 2022 at 8:47:13 PM UTC+5:30 mithlesh kumar wrote:
Kindly read WP22 instead of P91
On Saturday, December 17, 2022 at 8:15:23 PM UTC+5:30 mithlesh kumar wrote:
Dear team,

I have observed vanadium in heat analysis of p91 MTC  , but as per code vanadium is not showing in chemical composition table. Suggest is it acceptable or not if acceptable code reference please.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/21151b29-5972-4606-930c-0fc03e313713n%40googlegroups.com
.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...