you have to remove all the mixing between the stainless steel and the low alloy steel electode

Στις Παρ, 8 Ιαν 2021 στις 5:18 π.μ., ο/η ilkinhasanov <ilkinhasanov.91@gmail.com> έγραψε:
Gents,

Site Construction team has made mistake and perform  welding of dissimilar joint (Storage tank (A312 TP 316) to Deck of Module (Carbon steel)  with wrong Electrode (E8018-G).Consequently weld has cracked. Joint configuration was a fillet weld with 8 mm leg length. Leg of tank is 55mm height. Site team is going to cut leg of tank approximately 20-30mm.
 
I think weld decay can cause crack of weld metal. I just want get your advise, if  we will try to repair it, what is a length of need to be removed from leg of tank to get rid of from affected microstructure zone? if site team will cut from leg 20-30mm , it will be enough or not?



Best Regards,
Ilkin Hasanov

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/32cf7e5e-ce52-4876-85ce-a2ce8cf93f9dn%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CAKtOB%2B%3DBH40TFsaXcuSR5K_RS0E%3DwL%2BfXNe9Sh_OLGQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...