It depends on thickness and no of passes. Maximum may be 3 mm for all thickness

On Wed, Jan 13, 2021, 4:34 PM yerriswamy wooluru <ysprabhu@gmail.com> wrote:
You can make use of profile projector

On Wed, 13 Jan, 2021, 3:52 pm Babur Khan, <mbabur.bwp@gmail.com> wrote:
Dear Mr . Hani Nabil,
Its depends on several factors i.e. Material type (weld ability), thickness of material, welding Process and Heat input during welding. 
Generally for carbon Steel and normal thickness we take care  25mm area from weld Line to base metal.

Muhammad Babur Khan
Sent from my iPhone

On 13 Jan 2021, at 9:35 AM, Hany Nabil <eng.hanynabil20@gmail.com> wrote:

Dear All ,

Please let me know how to calculate HAZ size in Welding ? 
--


 Best Regards,

 Eng. Hany Nabil
 Senior Welding Engineer
 Petrofac
 Engineering and Production Service
 Egypt Mobile: 002-01225622022




This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmTroonhdS%2B3fn0qZqnH%3D8MH6tDNZRhxvQj1oiM7BWLeTg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3A25CA16-5EE0-431A-8322-4CC58FA7B7B4%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFU4egq9KFJOpm40XAsmD0owp5zO8JkeNcs4KazR7hBAH5EdiA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMNN9%2B%3DPKwtH21q7-3_beeDhJPQwbYmtuYNmfvkLxu2Vg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...