Re: [MW:31922] Difference between AWS D1.1 & ASME Sec IX

AWS D1.1. - This is for  welding qualification in structural  welding application
                     There are pre qualified WPS s. 
                     Refer respective  chapters for qualification.

ASME SEC IX - This is for welding qualification for pressure  pressure part to pressure part   and pressure  pressure part to non pressure part welding application.
PQR needs to qualify WPS 



On Sat, Jan 9, 2021 at 11:58 AM Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:
Dear all,
Kindly share the Difference between AWS D1.1 & ASME Sec IX, if available.

Thank you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2rz_WF%2BEKTwA2AAvFfartFgVncf%2BZ3ceGRsgejGRpJ9bw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3MGSaRUP-RW503z-gq7EbEYi_0wdfnC46vfCeEw3F8P_Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...