Dear Vishwas,
As per the client , the procedure is to be qualified based on API 1104.Can you please advice me on the base material selection for Procedure/Welder qualifications?

On Monday, January 4, 2021 at 6:21:43 PM UTC+8 Vishwas Keskar Welding Manager WELDING wrote:
S275 JR is basically  material used for Structural  application.
I hope  , your application also is for structures .
For welding qualification ,  you can use AWS D1.1  OR  EN 15614

AWS D1.1 is well accepted  by Clients .
You have to qualify procedures/ Welders.



On Mon, Jan 4, 2021 at 2:10 PM 'Anumiah Veera Jegan' via Materials & Welding <material...@googlegroups.com> wrote:
Dear experts,

The base materials to be used in the project are based on BS EN 10025-2 : 2004 Grade S275JR.Can I qualify my procedure based on API 1104?. If so,can you please advice me on the grade of the base materials which can be used for the procedure qualification?.

Thanks.

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6274779e-16d4-447f-9636-cbb818c9105cn%40googlegroups.com.

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8c4eae10-c8c1-4adf-8d25-d243f4d71e2en%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...