Dear Experts

Kindly suggest on below case

We have prepared proposed wps on the basis of that pqr was welded in one of the established classification society. Test coupon were sent in NABL lab... TPI witnessed the same...four side bend, two tensile and hardness conducted in the lab. 

All test pass however one of the bend test failed due to defects length more the 3mm.

Then we approach TPI for re-test from the original specimen as per ASME QW202. 1 (3rd para).

But classification society project manager says it is a wrong practice and we will witness only new welding samples. 

We told him that it is written in the code and if all other test are passed then failure is not related to welding parameters.... It is particularly related to specific defect may be present at that point and that has caused failure and for that there is an option for re-test as per ASME Sec IX. 

Kindly suggest your opinion... And what should we do now? Because classification society is not willing to witness the re-test as per ASME sec ix. 

Rgds, 
M R Gupta
+91-9820604076

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/137049239.5216646.1609653065444%40mail.yahoo.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUNnfm5%3D5c1euBjCWQgCzusNX72AFq3uJ9xy1CYtpR9iFQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...