Sunday, January 3, 2021

Re: [MW:31898] Continuous crack in forged duplex ring by PAW process

HI,

ER 2594 has both Austenitic & Ferritc  Str.   Better to do with ER 309 L Or ER 312 L 
Also Make sure Grind off all the fatigue Layer completely . Deposit with low heat Input .also slow cooling ( cover by glass wool / welding blanket)

Kr
Das

On Sat, 2 Jan 2021 at 17:41, SURESH <qms.pjgpl@gmail.com> wrote:
Dear Experts
Need all your experience sharing on the below problem.

Material: ASTM A182, F55
Process: PAW
Welding: Hard facing weld overlay
Consumable ERCoCr-B (Stellite 12)
Layer deposited: 2 Layers
Deposition thick: 3 to 4mm ERCoCr-B on Base material
Interpass maintained: 150*C

During weld deposition of PAW process on 2nd layer itself crack has been propagated. We tried to rework by grinding and touch up, from that moment crack has been developed. If we tried to attend the crack place, other place are developing crack. Also now we again tried to rework, crack has been developing all the place, kindly tell me where this goes wrong?????

We are confused to do rework. As we goes deep to remove the crack, so we tried to grind 4mm deep now again deposited ER2594 by Tig process and then we follwed to weld by ERCoCr-B filler by TIG process. Again crack is developing enormously.

Please give valuable input to overcome from where we goes wrong in this?


REGARDS
SURESH 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7aa85aac-7d40-4817-8c7e-4277f7865b76n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJyLdkpGu6AVdu8H6WVsyBFWMeQZswgKtEBDkTG56thmwnvRUw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...