Dear Experts, 

Good day to you all!

IF I make a PQR with 6G position, 
1- Can I prepare a WPS for 4G position & 6G position as well? 
2- 4G and 6G must be separate WPS's or it can be in same WPS?



And Can I prepare an ASME WPS with the same AWS D1.1 PQR if I cover all ESSENTIAL Variables?

If YES, I can cover all the required Mech Testings as per requirements of ASME.

If anyone has a sample please share it as a reference.(PWPS, PQR, WPS- Material P1, SMAW process)

regards
raj