Thursday, January 14, 2021

[MW:31930] Re: BUS beam

Fillet weld has to be done from both sides.

On Thursday, 5 November 2020 at 07:58:20 UTC+5:30 eng.bas...@gmail.com wrote:
Dear all

@ built-up section beam in welding SAW progress if the web Thk. equal or less than 8mm.
Can welding from one side only or I can't 

Thanx

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a32c9822-fd3b-49f1-960b-93ec5f9501e5n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...