Dear All Concern,

Please help me selection for welding of pipe materials as per following spec:

Pipe Spec: 

1. NB: 750 mm; WT: 25.4 mm; API 5L -X65M, PSL -2, LSAW, ASTM B36.10M

2. NB: 200 mm; SCH: XS; API 5L -X65M, PSL -2, SMLS, ASTM B36.10M

3. NB: 100 mm; SCH: XS; API 5L -X65M, PSL -2, SMLS, ASTM B36.10M

Minimum Yield Strength of Pipe : 450 MPa

Ultimate Tensile Strength of Pipe : 535 MPa

My client wants me to do GTAW for Root & Hot passes and SMAW for Filling & Capping Passes. 

I wish for everyone's sound health and sound mind. 

Thanks In Advance,

Md. Asif Al-Istiaque Chowdhury
Manager (Project Sales & Operation)
WhatsApp No.: +88 01925-884133

The Royal Utilisation Services (Pvt.) Ltd.
(An ISO 9001:2008 Certified Company)
House # 383 (3rd Floor), Road # 28,
New DOHS, Mohakhali, Dhaka-1206, Bangladesh.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/efaf3bef-3826-4097-bf55-d092c6c0850an%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...