Saturday, October 31, 2020

Re: [MW:31660] Allowable tolerance

Review the following:

ASME 36.19
ASME B16.9
ASME B16.11
ASTM A960

Cheers.....

On Sat, Oct 31, 2020 at 7:09 AM Dhaneesh p <dhaneeshdotp@gmail.com> wrote:
Dear experts 
my query is , what is allowable tolerance in length , diameter , thickness for material receiving inspection of following ( please mention reference code   )
1) pipe ASTM 312 TP 304  , SIZE 3/4" , THK : 2.87 mm , Length : 6 m 
2) fittings  ASTM A 403 WP 304 , THK : 3.38
Regards 
Dhaneesh 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bda38b20-5a5b-4094-9d28-2b8a410fa53cn%40googlegroups.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUNRR8aZvqRNxE%3DQpYMAVNVGAJ_jvajhL8_8W7yu99zx6Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...