Dear Sir,

You can put Diameter : All in WPS because the diameter is non essential variable.

Also, for welding qualification as per ASME-9 QW-400 not QW-200 (since QW- 200 for welder qualification).


Thanks & Regards
Hany Nabil 

On Sat, Oct 31, 2020 at 8:55 AM NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> wrote:
Dear Experts,

Greetings of the day.

I have a doubt regarding the WPS preparation. 

I have prepared one PQR of GTAW+SMAW in P22 material of size 6 inch.


But in wps the qualified diameter what I should write as per asme sec 9 , qw-200.


Is this can qualified for all the diameter?
Should i need to write any diameter range in wps.


Even though the thickness range is 5 to 2T.

Experts please advise me.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6c9cd6e7-1d3d-426d-adb7-d361351c767an%40googlegroups.com.
--


 Best Regards,

 Eng. Hany Nabil
 Senior Welding Engineer
 Petrofac
 Engineering and Production Service
 Egypt Mobile: 002-01225622022




This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmQ%3D1TeVV3hx1fDYP8eHmBfgUJCTzEbXoCi2u_pEMVkEqg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...