Post Heat is applicable to bake out Hydrogen before delayed PWHT. When Flux bearing welding process, like FCAW, SMAW, SAW ect  on Higher thickness ( Multiple layers) and Alloy steels to avoid Delayed Crack/ HICC

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Oct 28, 2020 at 10:41 AM udaya bhaskar <dusroni@gmail.com> wrote:
Mr.Nikhil,
Post Heat applicable at,if you done any welding activity after PWHT.


On Mon, Oct 26, 2020 at 7:41 AM NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> wrote:

Dear sir, Good evening

Sir, kindly please  solve my doubt related to POST HEATING IN PWHT.

1.Where we need to do post heating.

2.If I am doing pwht sudden after welding is there any need of post heating or not.

3.In any code post heating mentioned.

Please give me answer for the above mentioned question.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5d07c2d7-f780-459d-8aab-53e92469c23cn%40googlegroups.com.


--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RMwyXqwdbPS5%3DGPKqT6TkE4rnAO6SzoXgCxEj_Kj9isTg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePuadOGch9nJCsSdB2W79199MTPOF0GG%3D_9tki6w3TkKA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...