Hi,

Design calculations will let you know if it is due to over pressure,

Regards 

On Tue, 27 Oct 2020, 15:45 Muhammed Ibrahim PK, <ibratech@gmail.com> wrote:
Gents, 

Is there any option to find out if the vessel is cracked because of over pressure at site by mistake. 

If we perform a tensile test across the crack area, can we get any clue if grains are already permament deformed due to over pressure? 

Or is there any other metallogaraphic method can we employ? 

Reg, 
Ibrahim

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmOdwJJ9v2kp-NWhkvQsj89n_9c1nNh5P_hJk_csUEmz%3Dg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp_tDfmNV4Ox%3DvWd8PTTs4%2BXH%2BU4FuLhhX_J%3Dh8V_taSEA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...