Hi,
Nornally for Saudi Aramco projects we need to 3 cycle simulation PWHT tested plates.
PQR also need to test for one cycle as well as 3 cycle.
Reg,
Ibrahim
On Thu, 22 Oct 2020, 3:14 pm Zacharias Rohith Joseph, <rohithjoseph18@gmail.com> wrote:
Hello,Can someone pls guide on how many times PWHT can be repeated on a weld and the requirement of PWHT for joint which have been repaired post PWHT.If there are references in other codes that you know of you may pls quote that too.Thank you--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/79e76538-eb77-4600-80d9-67389e9d72a1n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmO-gpAjitbew5jjXw_WWXUVhkM8GFjD8ac-NbL3-nwS0A%40mail.gmail.com.
Comments