Monday, October 26, 2020

Re: [MW:31619] POST HEATING OR dehydrogenation heat treatment

Mr.Udaya bhaskar,

Sir, QW-407 Gives description about PWHT. There is no mention about post heating or DHT.

BEST REGARDS,
NIKHIL THOMAS JOY
IWI LIMITED 
ADNOC-WHRP
0544975526


On Mon, Oct 26, 2020 at 1:06 PM udaya bhaskar <dusroni@gmail.com> wrote:
FYI,

Check
 QW-407

On Sat, Oct 24, 2020 at 5:06 PM NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> wrote:
Dear friends,

Greetings of the day,

I would like to check the post heating details for pipe welded joints for alloy materials.
Please share in which code its available to refer.

My main concern , there is any need to mention post heating in wps or pqr.
if yes, in which code its mention.

Waiting for experts advice.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/65d036c8-f83f-4f11-8254-1ebbfb28f8d0n%40googlegroups.com.


--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RMuOavVPZFa36L65xiTT4nPgMLFfNASHVGPoXOKDZS7gg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJxkuiU8Q-56ZeJkK2G2KC7d1roTBryrT11mj6Firb-cyrZ25g%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...