Sunday, October 25, 2020

Re: [MW:31612] Alloy 20

Yes 
you can use 

use ER320LR 



Regards

On Fri, Oct 23, 2020 at 8:03 AM Solai Murugan <solai.kg@gmail.com> wrote:
Dear sir.
Alloy 20 material Uns no8020. Which filler wire suitable?? Can I use ER320 Filler wire.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHPVRABrExyjtT6XWp5Z7vR61VrfxbB7X%2Bg%3DWac-XOiScECVdQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NcbaXsm%3D2dkJeXsb8GfhSq8pEXxNx03iMXNCfATMtYMg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...