For welding qualification ( WPS )
You have to follow ASME- IX , not ASME VIII

Thanks & Regards,

On Sat, Oct 24, 2020 at 6:59 AM K K <karan.hbl@gmail.com> wrote:
Dear Experts,

Please refer below WPS and PQR details.

PQR Details - Base Metal - ASTM A106 Gr.B  To ASTM A106 Gr.B. ( P No - 1 Gr.No - 1 To  P No - 1 Gr.No - 1 ).
Process - GTAW  + SMAW ( GTAW - 4.8 mm + SMAW - 13.46 mm)
Thickness of the Coupon -18.26 mm, Dia - 6"
With PWHT - 638°C ,time 72 min.
No Impact tested.
DESIGN TEMP. / MDMT (°C) -290 / 5 .

WPS Details - Base Metal - ASTM A106 / A516 Gr.B / Gr.70  To  ASTM A106 / A516 Gr.B / Gr.70 . ( P No - 1 Gr.No - 1/2 To  P No - 1 Gr.No - 1/2 ).
Process - GTAW  + SMAW ( GTAW - 9.6 mm + SMAW - 15.4 mm).
SFA No- GTAW - 5.18 and for SMAW - 5.1.
AWS No - GTAW - ER70S-3 and SMAW - E7018-1H4R.
Pre heat - less than 12.7 mm -10°C and less than 25 mm 75°C.
Inter pass Temp. -315°C.
PWHT - 620°C, Holding time 1 hr thk +1 hour min.

According to above details help me to review, as per ASME Section VIII for Boiler and Pressure Vessel Code.
And I need your suggestion what are the essentials requirements according ASME  Sec.VIII. And what are the important things i have to check.
Please suggested me with clause reference.

Please send me your valuable suggestions, it's Supports me lot.

Thanks and Regards
Kiran




 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c3e78183-f533-400b-bfe1-ba8e24f94c6an%40googlegroups.com.
--


 Best Regards,

 Eng. Hany Nabil
 Senior Welding Engineer
 Petrofac
 Engineering and Production Service
 Egypt Mobile: 002-01225622022




This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmSsDQqPOy0XJ__uyHX3_zaKxz5bo0QnO4drHd_ybGYzKw%40mail.gmail.com.

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...