Hi,

In most Ni alloys ( ASME II B-N625,825,8020 ) filler wire is used ER NiCrMo-3 , Ni-58,Cr-23,Mo-10 maximum.
ER 320 has chemistry Ni-36 , Cr-21, Mo-3 max only, so it cannot be used for Ni alloys.

Thanks and Regards,

Sivakumar. K
+971-522960995.

On Fri, Oct 23, 2020 at 8:03 AM Solai Murugan <solai.kg@gmail.com> wrote:
Dear sir.
Alloy 20 material Uns no8020. Which filler wire suitable?? Can I use ER320 Filler wire.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHPVRABrExyjtT6XWp5Z7vR61VrfxbB7X%2Bg%3DWac-XOiScECVdQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADNtOzKATbSq87Lwt4dTuFu2VpEEgGj5oD0upWKogQ_U_YFK3A%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...