Re: [MW:31591] welding activity pipeline

Hi,

There is no issue here, Root & Hot passes are essential variables at piping.
You can do.

On Thu, Oct 22, 2020 at 2:58 PM dorh <dorrihriz@gmail.com> wrote:

Hello ;

We work for welding activity pipeline 12"         X52       thickness 8.38 mm

Root / hot pass      GTAW

Filling / cap            SMAW

In order to optimize production Contractor propose to proceed with GTAW  first ,   for example for he weld  first 10 weld joint GTAW  after that he come back tomorrow  with and filling and cap  weld joint with SMAW.

 

It's some issue for that    ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/386e7357-4115-479b-b8bf-45df08b78becn%40googlegroups.com.


--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM46AZv6-JgUUi4mZuJDTD%3DE5Ys7avJS-AKxOgvJo8BPg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...