Wednesday, October 21, 2020

Re: [MW:31580] Query related to WPS

Yes, it is correct, for non impact applications. When impact requirement applies, group number becomes essential.

On Wed, Oct 21, 2020, 6:12 PM Manish Kumar <mkmkr431@gmail.com> wrote:
Dear Sir,
If P number of material 1 & group number 1 & 2 is mentioned in WPS.While supporting relevant PQR is P number 1 & group number only 2. In this case,Will WPS be valid for relevant PQR.

Please advise us .

Attachment-
WPS & PQR 

--
Regards

Manish Kumar
Inspection(Mechanical) Engineer
PDIL-HURL Barauni site

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k78r-LmTKgXVDyMf_9wE9PtMAo_C8QBbsd6aqpTaHWgwg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFS9gDMBowiLqX8_a-AWw%3DJfZtKgiewFDtyWk7y7%2BV1M_8hkwg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...