20 cm are quite long and the heat affected zones will not overlap.
The weld has to be performed with a WPS which will include:
preheat at 90 degC
Mutipass welding with low hydrogen process
Temper bead which will be grinded flush with base metal.
Then perform RT

Στις Δευ, 19 Οκτ 2020 στις 6:30 π.μ., ο/η basem elabd <eng.basem.elabd@gmail.com> έγραψε:
Dear all

During built-up section beam assembly, if the upper flange is short, is it possible to connect a link of length 20cm and what minimum length can be connection

Thank you 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACct1WGdoBH1em8JzJaujEOt1KuWseuOm_J01hQajhLoZv9Rbw%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CaQJjPeK%2B1FKJv6mkEUvC-wy%3D733MXeBwZbHicLtq_7A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...