Dear  Vinoth / Experts 

i had prepared preliminary WPS as per  ISO 15614-1  so please check all parameters and inputs are ok or not 

additionally , check if this cover welding positions up to 6G and steel grade S355 and thickness up to 32mm 

Appreciate your fast action and assistance 

Regards,
H.A

On Sat, Oct 17, 2020 at 7:40 AM Hani Al Masry <hanyonalfy@gmail.com> wrote:
 
how about 

·                  BS EN ISO 15614-1 Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys


what is the major changes i need to made to the current WPS to convert it from AWS to 



On Fri, Oct 16, 2020 at 7:29 AM Vinoth Rajendran <rajvinoth1987@gmail.com> wrote:
Please go through EN  ISO 15609, EN ISO 15614-1, EN ISO 9606

On Thu, Oct 15, 2020, 18:47 Hani Al Masry <hanyonalfy@gmail.com> wrote:
Dear Experts 

Our client is asking to convert our WPS from AWS to BS Standards
can you please advise 
which BS standards we need to use 
what the mean steps to be changed according to this BS 
Requirement of back stip for pipe welding 

Regards,
H.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzfjuGE1OGLGRz%2B7gY0syR5F8ifC9jRFWdyzzR3n7bZDXA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Ba0BHbLE%2BRtObsF4XaaMcen325c4QbBTeGs4DK5VDC%2ByeQV%2Bg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzeQ36kA5njY74o4nv-c8QPGy7mmKGc4XywouR3mbmCFEg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...