Please go through EN  ISO 15609, EN ISO 15614-1, EN ISO 9606

On Thu, Oct 15, 2020, 18:47 Hani Al Masry <hanyonalfy@gmail.com> wrote:
Dear Experts 

Our client is asking to convert our WPS from AWS to BS Standards
can you please advise 
which BS standards we need to use 
what the mean steps to be changed according to this BS 
Requirement of back stip for pipe welding 

Regards,
H.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzfjuGE1OGLGRz%2B7gY0syR5F8ifC9jRFWdyzzR3n7bZDXA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Ba0BHbLE%2BRtObsF4XaaMcen325c4QbBTeGs4DK5VDC%2ByeQV%2Bg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...