Yes you can as per ASME section ix
On Tue, Jul 7, 2020, 17:03 'wilfred kojo' via Materials & Welding <materials-welding@googlegroups.com> wrote:
--Hi,You can use since both P-nos and Group nos are the same.On Tuesday, 7 July 2020, 06:29:16 GMT+1, Dharma dattu <dharmadattu@gmail.com> wrote:Hello All,--We have a new project for which main components are SA 312 TP 304L material, currently we have SA 312 TP 304 WPS can we ues the same, as the Pno. is same!Regards,Dharma Dattu. B
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/89ae66ad-2aad-40ce-aed3-fe009c801617o%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1361238169.6457761.1594120439406%40mail.yahoo.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOBQNgFuzR%2BOwbkWx2-nne0G3%2BDdZe6ZKQCY-Owa63QcA%40mail.gmail.com.
No comments:
Post a Comment