Re: [MW:31115] SA 312 TP304 for SA 312 TP 304L

Okay. But consumables should have L Carbon

On Tue, 7 Jul 2020 10:59 am Dharma dattu, <dharmadattu@gmail.com> wrote:
Hello All,

We have a new project for which main components are SA 312 TP 304L material, currently we have SA 312 TP 304 WPS can we ues the same, as the Pno. is same!

Regards,
Dharma Dattu. B

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/89ae66ad-2aad-40ce-aed3-fe009c801617o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN44duCjVm3MfVN1hX8m05aKk3O_biKK4-nnjRvppH80g%40mail.gmail.com.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...