Hi!
However what are the requirement?
Like
Impact test temp.Thk of weld n plate.Process being used . PWHT tem n time  consumables used
On this basis you can decide parameters and  precautions to be followed
Regards
Hegde



On Sun, 19 Jan 2020 at 7:29, Revdiwala Darshan
<darshanmrevdiwala@gmail.com> wrote:
Dear Experts,

Can anyone suggest welding consumables for welding of SA 537 CL 2 ?

And precautions during welding.

Thanks,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABDq6ghMxsVcLvE9XAqhUQutToi5dP8_-x30A6RdUcjKdpzSfg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1239338402.2908207.1579405972304%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...