Re: [MW:30353] PWHT For Trunnion support

No need, pls refer governing thickness specified in B31.3

Regards,

On Sat, 4 Jan 2020 at 8:37 PM Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear Raghuram Bathula,

   The main run pipe 20" is having thickness of 31.mm and being subjected to PWHT.
A dummy leg (12") is welded to the main pipe as dummy leg. pls confirm that, do we require PWHT at this joints as highlighted in below snap


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zOsMaca5bYCPWfVvRa1kRdBWqgcGKGMNEXf_k_dMXzMg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_6cSezddAR5BYWxvufNWNcF3nNVeAfqx12%3DbFqDiBvL-K1TQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...