Re: [MW:30378] Hardness after PWHT

Hi
Generally BHN235 MAX is acceptable limit after PWHT
Regards
Hegde



On Tue, 14 Jan 2020 at 17:28, patelroshankk@gmail.com
<patelroshankk@gmail.com> wrote:
Dear Experts please explain what hardness of Weld, HAZ, Parents metal is acceptable for F11 & F22 after Post weld Heat treatment.

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/22949c81-66b3-46b2-bd4a-5a46a78bc6d2%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1689425833.9532873.1579015447056%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...