I have been in several ASME audits for recertification (Joint Review), with Designers U, S and R of the National Board, with the Authorized Inspection Agencies: OneCis and HSB GS and certainly non-Dstructive Testing Procedures are presented in these audits, such as VT, PT and others, and in none of the cases did these procedures carry signatures of a Level III of ASNT.
He estado en varias auditorias ASME para recertificación (Joint Review), con Designadores U, S y R del National Board, con las Agencias de Inspección Autorizadas: OneCis y HSB GS y ciertamente se presentan Procedimientos de Pruebas No Dstructivas en estas auditorias, como son VT, PT y otros más, y en ninguno de los casos estos procedimientos llevaron firmas de un Nivel III de ASNT.
El jue., 9 ene. 2020 a las 5:13, Kannayeram Gnanapandithan (<kgpandithan@gmail.com>) escribió:
Mainly required for stamp holders whether it is coded or non coded. All NDT procedure and personal are to be certified/ approved by Level 3.--On Thu, 9 Jan 2020 2:38 pm chiluka venkatramulu, <ramuluchiluka@gmail.com> wrote:Dear All,--Pl clarify whether it is required NDT Level-III approvals for all NDT procedures? or required only for coded vessels.Pl specify the code requirement.Thanks & Regards,Venkatramulu CH
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdHdFX5ePVY4%2B5GB9pFh4ZGGoRu0ntafcZrkCw17XMdkrQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM4VRRfT57r-k4nyacd9PjZftwsP1V38bMVu%2B3swydHZg%40mail.gmail.com.
Ing. José Juan Jiménez Alejandro
Independent Consultant in Parts
and Pressure Equipment
SSI-TPI
Móvil +52 1 812 352 4606
Skype: jjjimeneza
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurK-ubnnur2t%2BsL1bKa%2BEWc_DNZ8%2B04RV4L3yV0CiLc-eQ%40mail.gmail.com.
Comments