Friday, January 17, 2020

Re: [MW:30397] Re: P8 material limit of as per QW-403.6

The P8 does not require PWHT

El jue., 16 ene. 2020 a las 21:17, JAYAPAL DHAKSHNAMOORTHY (<jmoorthy191@gmail.com>) escribió:
Our MDMT is -45 degree

On Tue, 14 Jan 2020, 10:08 ABHISHEK SINGH <mech.abhi17@gmail.com wrote:
As per QW-403.6 thickness limit will be 3 to 12 mm.
But in yours case what is the MDMT?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/382ebed6-b215-4dff-abcc-5c5bcfafe0b8%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHHcqJczsicoZGb0oznA8QfuPHNyQczYZX8LsjENtuymOfUW%2Bg%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJy94zRofq29OgA981WtLyzoeANLUACF83Li%3DBmsF7rcQ%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...