it is recommended to use the long seam weld shall be 90 to 180 degree orientation between two pipes. it helps to restrict crack  propagation during failure. 

On Wed, Jan 15, 2020 at 4:50 PM Durgesh <durgesh.gaonkar@galiakotwala.in> wrote:
please refer attached sketch for better understanding.,

Pleas suggest permissible welding procedure with reference ASME standard. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e8c953fc-6602-4c81-9ccc-329d270235a7%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEXs1KqXmuT6u6a7SJ_dES2LPX9j7i9mxpN%3DBy%3Db7n9bu1j39w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...