Dear Sir,
Please refer Table 323.3.1 of ASME B31.3.
Please review.
Regards,
Hareesh K V
On Mon, Jan 6, 2020, 9:29 AM José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
Good morning and greetings to all, dear colleagues and specialists on the subject.
You can cite the paragraph of ASME B31.3 where you specify that the maximum thickness is T + 6 mm, thanks in advance.
El dom., 5 ene. 2020 a las 8:12, Hareesh K V (<hareesh.kitco@gmail.com>) escribió:Dear Sir,For the condition with impact testing,The minimum thickness requirement is as per ASME BPVC Sec IX is 3 mm.The maximum thickness as per ASME BPVC Sec IX is 2TBut the maximum thickness as per ASME B 31.3 is T+6mm.Regards,Hareesh K V--On Mon, Dec 30, 2019, 11:05 AM JAYAPAL DHAKSHNAMOORTHY <jmoorthy191@gmail.com> wrote:--Dear experts,I have qualified PQR of Thickness-6mm (P8G1) Austenitic stainless steel, & What is the minimum and max.thickness qualified as Per QW-403.6.in WPS (for Impact).Regards,DHAKSHNAMOORTHY.J
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHHcqJdo7f3JVp4vAkH-77ucP9Gt4Z4uSVNmsM0o%3DfTr72cuXQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEv1fk8uRMFXdsiukUNJ5cs4i7QZGRRPziR_NPHRAA5a3-FEPw%40mail.gmail.com.
----Ing. José Juan Jiménez Alejandro
Independent Consultant in Parts
and Pressure Equipment
SSI-TPI
Móvil +52 1 812 352 4606
Skype: jjjimeneza
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJQ3o0tpOVt0rZOTNG_SWqq3JHvbWgVMjtLomwqFs4qmQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEv1fk_5Pd1Chj0JDcbz9ouipBbLgGO0etipQGH4-XDBbCv_zA%40mail.gmail.com.
Comments