Re: [MW:30373] Welding Parameter for HP modification (25Cr-35Ni-0.1C+Nb) Material

Any interpass temperature restrictions

On Tue, 14 Jan 2020 2:39 pm 'Karthik' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Hi,
Go with ENiCrFe-2 (Incoweld A) or ENiCrCoMo3 (Inconel 617). No PWHT needed. You may preheat up to maximum of 75 degree Celsius.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282

E-mail : karthik6684@yahoo.com



On Tuesday, January 14, 2020, 03:51:56 PM GMT+7, <tuanpvecc@gmail.com> wrote:


Dear Experts 
Please suggest a good welding parameter for HP modification (25Cr-35Ni-0.1C+Nb) Material 
Welding consumable, PWHT if need.

Thank you 

N.A. Tuan


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/525e8e0a-6c8b-4f00-bc35-f83b20bbb085%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/105142528.7421479.1578992924882%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePEYp13k%3DQHPpsQkQDuCRcG58kkoKaP4_6VGJfLpKHG0w%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...