La ovalidad en Recipientes a Presión es 1%, bajo ASME VIII Div. 1; en dobleces de tubería es un 8% de acuerdo al PFI Standard ES-24: PIPE BENDING METHODS, TOLERANCES, PROCESS AND MATERIAL
REQUIREMENTS, en codos no lo se, pero en tubería generalmente es el 1%.
Ovality in Pressure Vessels is 1%, under ASME VIII Div. 1; in pipe bends it is 8% according to PFI Standard ES-24: PIPE BENDING METHODS, TOLERANCES, PROCESS AND MATERIAL
REQUIREMENTS, in elbows I don't know, but in pipe it is usually 1%.

El mié., 15 ene. 2020 a las 5:20, Durgesh (<durgesh.gaonkar@galiakotwala.in>) escribió:
What is the permissible Ovality in Pipe to Pipe or Pipe to Elbow for welding ?, what type of welding can it be compensate it ? and reference of the ASME std to follow.
e-g) i got the ovality of 5 mm radial between O.D of pipe and elbow of 500NB (OD 508mm).

Please suggest so i can convince my customer. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01c9bbd7-d465-409c-b41d-387fd0009766%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJ7QxOJT%2BPXtKBaDEuP9PtFWC7hC2jXk3JwC33Rv%2B%3D1nA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...