[MW:30365] Re: how to verify the weld joint integrity without destructive test-reg

the on site metallography can help us in this situation.

Thanks&Regards,

G.K.PILLAI.

MOBILE

+97433329545    (QATAR)
+919500755882   (INDIA)

On Wed, 8 Jan 2020, 09:07 G.K.PILLAI, <pillai762000@gmail.com> wrote:
dear experts,

 can we have to verify the structural weld joint integrity with any one of non destructive test methods.( exactly my question is here  during welding  the contractor  may not be following the preheat and intrepass temperature .but the weld was completed.in this situation how to verify the weld joint integrity without destructive test)

Thanks&Regards,

G.K.PILLAI.

MOBILE

+97433329545    (QATAR)
+919500755882   (INDIA)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACmDAmWjMCWE9H%3DGaQivJCXftd%3DykYjMm8Ni8Jv1qa5ZiUnm%3DQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...