Re: [MW:30346] PWHT For Trunnion support

If the material is CS as per B31.3, preheat temp is above 95 degree centrigrade then no need to conduct PWHT.
Only you have to qualify PQR

On Sun, 5 Jan 2020, 13:58 Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
Governing thickness is as per B31.1 & 31.3 is Nominal material thickness??

On Sat, 4 Jan 2020 9:50 pm Tajuddin Mohammed, <tajuddinjntu@gmail.com> wrote:
Yes we need to do the  PWHT of these type of joints as it is directly welded to the pipe

Mohammed Tajuddin

On Sat, 4 Jan 2020, 6:07 pm Chiranjeevi A, <chiranjeevipuvvula@gmail.com> wrote:
Dear Raghuram Bathula,

   The main run pipe 20" is having thickness of 31.mm and being subjected to PWHT.
A dummy leg (12") is welded to the main pipe as dummy leg. pls confirm that, do we require PWHT at this joints as highlighted in below snap


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zOsMaca5bYCPWfVvRa1kRdBWqgcGKGMNEXf_k_dMXzMg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACZrEUbwy%2BdLw1gP70k18Ox6iPs%3DngfQmjzpqYG9xiWw44kXCA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOCE4j5Tb80xvgijR5mXNnOHUsMuS_jdLXhT8fTOMxMOA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8moJ%2BCiar3Jei5W2R3jrzGhELKaa82WtQ97yGeTP3Vjfg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...