Re: [MW:30381] P number for SA387 Gr 9 plate for PQR qualifications

Please review Table QB / QW-422,   ASME Section IX.
Greetings!

El mar., 14 ene. 2020 a las 21:21, satheesh kumar (<satheesh.psk123@gmail.com>) escribió:
Dear experts,...
I need to qualify a PQR for SA 335 Gr P9 pipe welding. We have plate SA 387 Gr 9.
But I don't find P number allocated for SA387 Gr 9, and UNS number is matching. Can we consider the P number as 5B?
Someone may object that it is unlisted material??
Please advise and share your thoughts on this why this particular plate grade is not listed in p number table.
.
With regards, 
SATHEESH KUMAR.P 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOX%2BP-vWLeYMzcVvFGukWKcpXU4BFF0c-rNidsBiFNNBLdU3SQ%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BjrP5MvuGjOFJR_zid%3DRGz8hKvrQbd6g0ixGy%2BFufFDg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...