Hi,
Inconel 625 is P.Number 43 and Inconel 825 is P.Number 45. So you can not use the WPS of P.No.45 to weld P.No.43. Please find below the extraction from Sec.IX

Inline image


Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282

E-mail : karthik6684@yahoo.com



On Wednesday, January 15, 2020, 12:46:11 PM GMT+7, Babu Chathoth <babu8803@gmail.com> wrote:


dear Guy's,

GM

The WPS which is qualified with P1 Gr.2 with Clad Alloy 825 will qualify to weld P1 Gr.2 with Clad Alloy 625 to equivalent or same material…? required separate qualification for  P1 Gr.2 with Clad Alloy 625 ?.


thanks in advance for your's prompt reply.


Babu 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9a533821-faa6-473e-be7f-15a39c2ffcc6%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...