Re: [MW:30399] P8 WPS qualification

Your question is not very clear to me, but I can tell you the following: If it is a P8 with another P8, you just have to verify that, that your WPS complies with the same P Numbers and with the same F Number and also with the Number A regarding your PQR.
Remember: P "+" F = A
With the data you present, my answer is YES, but I repeat, as you present it, it is not entirely clear to me.
Regards!.


El vie., 17 ene. 2020 a las 1:56, Kannayeram Gnanapandithan (<kgpandithan@gmail.com>) escribió:
Other than E309, it seems to be ok. For E309, check the A no. It may be A9 instead of A8. Pl check in Section 9

On Fri, 17 Jan 2020 8:47 am Muhammed Ibrahim PK, <ibratech@gmail.com> wrote:
Gents,

Please help to find the answer for below. Choices are given below. What would be the answer?

A repair organization has a WPS which states it is qualified for P-8 to
P-8 material welded with E308, E308L, E309, E316, electrodes (SMAW
process). The PQR, supporting this WPS, states the weld test coupons were
SA-240 Type 304L material, welded with E308 electrodes. Is the WPS properly
qualified for the base material listed?

A. Yes
B. No
C. Not enough information given
D. Yes, if properly heat treated

Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmNviEu9VaoJQjzFC3gz5ci1_AaJty1vnCukLYVpsTimPg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM6%3D2frntfP9SDc4sTcb-d%3D2Uxrkzc0Ni7bO_%3Dcg3uV%3DA%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BT7gwtXnrAbk-bWp%3DQEJFvZNBwvJyj1-1Noh7FKqZPMw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...