Sunday, January 19, 2020

Re: [MW:30407] Welder qualification

Hi, for WPS, position is not an essential variable. You can use WPS qualified with any position.

Karthik


Sent from Yahoo Mail for iPhone

On Saturday, January 18, 2020, 7:02 PM, udaya bhaskar <dusroni@gmail.com> wrote:

Good day all my dear experts,

Please clarify?

1). I have 3G P1 materials( thk 22 mm)WPS &PQR .
can I qualify for 2G,6G(dia 6")WQT on this WPS.

2).Possible to qualify 6G WQT on 5G fixed pipe WPS(Dia >24") thk 9mm

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RMUjPMW0Ud8weSRgarP5NrpSAhO2i7_hxRO3AH8V89snw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...