[MW:30386] What is the permissible Ovality in Pipe to Pipe or Pipe to Elbow for welding ?, what type of welding can it be compensate it ? and reference of the ASME std to follow

What is the permissible Ovality in Pipe to Pipe or Pipe to Elbow for welding ?, what type of welding can it be compensate it ? and reference of the ASME std to follow.
e-g) i got the ovality of 5 mm radial between O.D of pipe and elbow of 500NB (OD 508mm).

Please suggest so i can convince my customer. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01c9bbd7-d465-409c-b41d-387fd0009766%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...