Re: [MW:30090] Re: PQR for PTAW Process by ASME Sec IX

It is important that you mention what the Construction Code is

El mar., 24 sept. 2019 a las 4:48, Bien_ND / weldinginspections.net (<bck055@gmail.com>) escribió:
please run follow machine manual and consumable manual.
I did a procedure PTA with Dura-Metal as them instruction.


On Monday, September 23, 2019 at 10:24:23 AM UTC+7, sathis...@gmail.com wrote:
> Dear Experts
>
> I would like to know below query on preparation of PQR as per ASME Sec IX, Process: PTAW by hardfacing overlay by Stellite 6 Powder
>
>
>
> 1. What is the current, voltage, Gas flow and Powder feed rate need to be maintained for 10mm and 25mm thickness plate. To which standard and reference i need to refer.
>
>
>
> 2. What is the pre heating and interpass temperature need to be maintained for P.No: 1,8,4,5A, 15E and to which standard need to refer
>
>
>
> 3. What is the hardness requirement for P.No: 1,8,4,5A, 15E during testing PQR? Which standard is mentioned this requirement?
>
>
>
> 4. Chemical analysis is mandatory for Co base as per ASME Sec IX , Table QW: 453
>
>
>
> Kindly give your suggestion and feedback for the above doubts
>
>
>
> Thanks in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/26d6e35c-4e74-4687-a9b1-425343919b7e%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLugykWuW1QJrM2_-8eG0pJUu6jEr0XymRiR4N6SBXkEQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...