Re: [MW:30020] Re: Difference between Control thickness & nominal material thickness ( Para. 331.1.3(c)

No, Exemption on PWHT is based on Nominal thickness not control thickness.



On Mon, Sep 2, 2019 at 7:56 PM anhtrangnghieng <anhtrangnghieng@gmail.com> wrote:
Dear Gents, 

i understand that if control thickness less than 25.4 mm , preheat & PWHT is not required as per Code ? 

thank you. 

Vào Th 6, 23 thg 8, 2019 vào lúc 15:25 Kannayeram Gnanapandithan <kgpandithan@gmail.com> đã viết:
Nominal material Thickness as  Example--- Pressure pipe is supported by another pipe( non pressure part) is being welded, Pressure part pipe thickness is 20mm whereas non pressure part thickness is 10mm,  In this case Nominal material thickness is 20mm. This is my understanding
 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Aug 23, 2019 at 9:48 AM atul khatri <atul.mnnit@gmail.com> wrote:
Hello all,
Here in the particular case the controlled thickness at weld shall be 6 mm.
Now as per table 331.1.3, for P.No-1 , for all control thickness , PWHT is exempted only if preheat of 95 deg c is applied on nominal material thickness > 25 mm. Here nominal material thickness is defined as thicker of the materials being joined.

So in this case, preheat shall require before welding.

thanks & regards
Atul Khatri

On Tue, Aug 20, 2019 at 11:28 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Not only control thickness. 

On Tue, 20 Aug 2019 9:58 am , <pkraneesh@gmail.com> wrote:

Control thickness is the thickness of weld and Nominal material thickness is the thickness of material

PWHT Requirement is based on control thickness (Table 331.1.3)

Preheat requirement is based on nominal material thickness

Hope you understand


Raneesh pk

QC Engineer

UAE 


On Saturday, August 3, 2019 at 9:06:23 AM UTC+4, anhtrang nghieng wrote:

Dear Experts, 
Could you please advise me for following question: 
Which thickness , Control thickness or Nominal material thicness as defined in Para. 331.1.3(c), shall be used to determine whether PWHT required or not in case preheat of 95 Deg C is NOT applied ? ( P-No. 1)

image.png

For case below, in accordance with ASME B31.3 2016 Ed , PWHT is required or not when preheat of 95 Deg C is NOT applied ? 
image.png
Thanks in advance.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3f6c1bef-b00f-4eb1-b3e6-aad113643433%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO%3DbnwcvcX9k9pUq-aWvziPqFuxtx0sQX6JsWq5wbMqpA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeAF2DaWe%2BYDpKm8P_gS04w5ub-KUUDoo3SmxyYJunj2zw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePVMWCmAhf0bp%3D0RBBLh51%2BMH7vk1X-MaMsw2%3DzcQWaTQ%40mail.gmail.com.


--




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADOyxJjtcLoy%2B5Lk%2BhLjQ_fhDg75ariUyyA7vE-Z8SZoOKYdNA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeC8H3z8K2EbWZ3n_MUSQNRQgzy6RP7aBdk%3DfJaRJYV2VQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...