Hello everyone ,

I am confused between Pwht requirements .

We are manufacturing a base frame of size 15m x 5 m  x 3 m in H besm of size 305x305x118x20mm thk and in which different size plate used to weld on beam but 105mm thk is the higher size of plate. weld is type of fillet.

So i need to know which thickness consider for pwht requirement & heating ,cooling rate calculation.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/543b6857-054b-41d4-8f38-e8379b4b35c7%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp9RdVLbqmnL1mBiRT%3Dqc%3DJMDT%3DRxOEJsRyZ04_5KJvpow%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...