Re: [MW:29851] Regarding Weld area calculation for branch reinforcement as per ASME B 31.3

No, the calculations have to be based on the minimum fillet weld size given by the code

Στις Τρί, 16 Ιουλ 2019 στις 8:52 π.μ., ο/η atul khatri <atul.mnnit@gmail.com> έγραψε:
Hello experts,
As per clause 304.3.3 of ASME B 31.3 (Reinforcement of welded branch connections), Area A4 is the area of other metal provided by welds and properly attached reinforcement.

While calculating the weld area , the minimum value of tc=0.7 Tb or 6mm (1/4 in.) ,except that larger dimensions may be used if the welder has been specifically instructed to make the welds to those dimensions.



Now my query is -- 
In case if welder has gone with higher weld thickness and weld throat is coming more than 6mm, than the weld area for reinforcement should be calculated based on higher thickness or restricted to 6mm only ?

Thanks and regards
Atul Khatri

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeDck91TCVhuBVvm%2Bn3wsE5i%3Dhsc9yP3rB1-LCnMG2bVcA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40C%3Dwm7%2BRzmn4cgtLy-Aosiu2bAjFL_H1jBRKRRnQKNcHw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...